Chemical analysis low alloyed steel, excluding nitrogen

SEK 1540 Excl. VAT

Test methods

Complete chemical analysis of a low alloyed steel (Fe>85%, Cr/Ni<5%), using optical emission spectroscopy.

Standards

Optical Emission Spectroscopy (OES) according to ASTM E1086

Combustion analysis according to ASTM E1019

This method is accredited according to SS-EN ISO/IEC 17025. For details*:

http://search.swedac.se/docs/A001539-001%20Omfattning%20Lab%201636%20AB%20Sandvik%20Materials%20Technology%20Analyslaboratoriet%20170628.pdf

*If the sample needs remelting, non accredited analysis methods are used.

Elements that will be analysed

Al, As, Cr, Cu, Mn, Mo, Nb, Ni, P, Si, Sn, Ti, V, W, Zn, C, S

Concentration range

Sample dimension requirements

The maximum size of the sample in total is 100x100 mm and with a height of 80 mm. At least one surface of the sample must be flat and the flat surface must ha diameter of at least 15 mm. If your sample is bigger than required size you can ad extra sample preparation to your order. Please note that if your sample need remelting, as in the case of analysing wire, Ti and Al can not be guaranteed to be analysed.

Requirements of sample contamination

If your sample is in any way contaminated by any of the following; explosives, oxidizing, flammable, toxic or radioactive elements or is in any other way harmful, you need to make a request for quotation

Delivery time

Normal delivery, after sample has been received by us is 2-4 days. 

Request for quotation

If you have an inquiry that does not fit into any of our standard services please don't hesitate to ask for a quotation.